Application Procedure
- Flush all equipment with Amercoat 911 or Amercoat 12 before use.
- Mix to a uniform consistency.
- If needed forworkability, thin with Amercoat 911 up to 1.2 pint per gallon.
- Apply a wet coat in even, parallel passes, overlap each pass 50 percent to avoid holidays, bare areas and pinholes.
If required, follow with a cross spray at right angles to first pass.
- Clean all equipmentwith Amercoat 911 or Amercoat 12immediately after use.
Temperature Resistance (Dry) |
°F |
°C |
continuous |
200 |
93 |
intermittent |
250 |
121 |
See temperature limits for primer or coating used as first coat. |
|